  • Advanced Procrastinator
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 201
  • Joined: 16-December 11

Posted 20 May 2012 - 04:58 PM

I'm going to buy some mason stain test packs, and I'm wondering what color blue people like to use.

I will be using it to make colored porcelain. I've used Wedgewood 6310 with good results, but it comes out on the slightly purple side.

Thanks


0

#2 User is offline   Fuad Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 14
  • Joined: 27-October 11

Posted 20 May 2012 - 06:15 PM

hi matt,

I use Zircon Blue (Mason 6315) that I get from Pottery Supply house in Canada.

Depending on how much you use, you can get a nice medium blue from it.

I cant find a picture of it where we used it though or else I would share.

Hope this helps
0

#3 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,359
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 20 May 2012 - 07:46 PM

I use Mazarene Blue ... It goes from deep blue to a lovely faded denim color as you add white clay.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#4 User is offline   macdoodle Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 75
  • Joined: 08-April 11
  • LocationOrange County, CA, USA

Posted 21 May 2012 - 12:25 PM

I've used colbalt oxide , it's a very vibrant blue. A little goes a very long way.
0

#5 User is offline   CatherineCory Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 21-May 12

Posted 21 May 2012 - 02:14 PM

I've used MS Robin's Egg with a low fire porcelain clay body. It fired to Cone 6 and maintained a light blue that was true to the color of the original stain material.I was awhile ago, but I believe I used 7%.
0

#6 User is offline   Karen B Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 88
  • Joined: 11-September 10
  • LocationMassachusetts

Posted 22 May 2012 - 07:00 AM

[quote name='CatherineCory' date='21 May 2012 - 02:14 PM' timestamp='1337627652' post='17369']
I've used MS Robin's Egg with a low fire porcelain clay body. It fired to Cone 6 and maintained a light blue that was true to the color of the original stain material.I was awhile ago, but I believe I used 7%.



Just a note that a few years ago I noticed that the Robins Egg changed. So please test any of these suggestions before making an investment.
0

#7 User is offline   Matt Oz Icon

  • Advanced Procrastinator
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 201
  • Joined: 16-December 11

Posted 22 May 2012 - 11:52 AM

Thanks for all the suggestions.

I know cobalt is the most common for blue, which is used in mazerine, but I see lighter stains use vanadium with zirconium.

I'll order some samples of mazerine and the others, then do some tests. It looks like Mason Color Works used to blend a cobalt containing stain with a vanadium, to get bright blue. I'll have to try that too.

Thanks again.