Dear All,
I just wanted to let the forum know that I while I had trouble with my kiln wash over the cold winter, I found that by putting a new shelf that I ordered in my oven @ 170 degrees for three hours and then apply the wash, I was good to go! Now all I have to do is bake this shelf with my next bisque fire.
I remember someone told me on this forum they bake their shelves in the sun before they put on the wash. Well, just know that it works. I had no bubbles, no cracks, nothing. It went on smooth, smooth and smooth.
Nelly