Just curious what clays and how many different clays people use.

I only use one type, #60 Laguna Brown with grog for pottery. This is the only clay I know.

Occasionally I use a Black clay (Stone Mountain) for some jewelry.
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 15 May 2012 - 01:09 AM

For production pottery-daves porcelain-white body
for flat pressed items-1/2 and 1/2 Thats have Daves porc and half WSO-white body
for large pots B-mix-white stoneware
for huge fish WSO-white body/ or big white

for salt pots-wood and sagger-stone ware
quayle sandstone buff-stoneware
rods bod-and just about any stoneware body laguna makes
I think I have about 6 others as well for salting
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   timbo_heff Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 61
  • Joined: 24-April 12
  • LocationMA / NY

Posted 15 May 2012 - 07:48 AM

I like to use a bunch of different Sheffield Pottery bodies:
Sheffield T1 and T3 and Wood Light stonewares for cone 10 ... sometime the screened versions, sometimes unscreened for a bit more iron play.
95400 grogged and no grog depending on size of piece for a white stoneware, good for my cone 6 electric glazed ware and also for 10 in wood and/or soda.
Ben's Mix for maximum flash helmer porcelain for wood.
and the Elaines cone 10 porcelain (wonderful thrower) for cone 10 gas reduction

0

#4 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,500
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 15 May 2012 - 07:55 AM

I use terra cotta, raku, raku paper clay, Frost as Armadillo Porcelain, Coleman Porcelain for saggar firings.
Marcia
Marcia Selsor
0

#5 User is offline   Denice Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 470
  • Joined: 02-April 10
  • LocationWichita, Kansas

Posted 15 May 2012 - 08:27 AM

I use terra cotta, several different Laguna C6 clays and I special order in different clays for projects that I am working on. I used to make my own clay but now I just get it premade and reclaim it. Denice
0

#6 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 15 May 2012 - 08:07 PM

The ones I use most often: Highwater Little Loafers (^6), Standard 266 Dark Brown (^6), Highwater Hestia (^10) and Standard 104 with and without grog (^05). On occasion dabble in others -- Highwater Buncombe White (^6) and Loafers Glory and Phoenix (^10), Standard 380 (groggy red clay for handbuilding and firing at ^10), Standard 112 Speckled Brown (^6). I inherited the Hestia from another potter who was moving. If you can find it, Campbell's Red Knob is an awesome body for ^10.