tile production I'm looking to 'farm out' 4.25"x 4.25" decorated t

#1 User is offline   longagopotter Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 14-May 12

Posted 14 May 2012 - 10:38 AM

I am a long ago ceramic graduate and now living in the Virgin Islands for a garment painter. His designs are delightful. He has recently expressed interest in offering 'standard' size 4.25x 4.25" tiles. My first attempts of researching sources is taking me to sentimental tiles ie photo transfers of the cute children or pets of your life- pricing 4x 4" at $13. ea! Not at all what we are looking for. Can someone suggest how this small business can have half a dozen tiles made in production?
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,378
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 29 May 2012 - 05:38 PM

6 tiles is not worth many folks time-the 13$ seems fair for custom work of 6 tiles to me no matter what size they are.
I'm a production potter not tile maker but have made tiles before

I long ago stopped taking custom orders as they where not worth it-6 tiles falls in that category for me.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 29 May 2012 - 07:38 PM

Excuse me but six tiles is not really production. Did you mean six tile designs to be put into production or literally six blank tiles?
INRI
0

#4 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,378
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 29 May 2012 - 08:59 PM

Ok after reading Lucille's post I may have misread your six tiles
If you want a true zillion production run of 6 designs heres a custom Tile shop I checked out a few years back and they do custom work.
They can handle your job as they fire 10 kilns 7 days a week.
The cost may be high but the quality is high
They are in Silver city New Mexico
Mark

http://www.syzygytile.com
Mark Cortright
www.liscomhillpottery.com
0

#5 User is offline   longagopotter Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 14-May 12

Posted 01 June 2012 - 08:25 AM

View PostMark C., on 29 May 2012 - 08:59 PM, said:

Ok after reading Lucille's post I may have misread your six tiles
If you want a true zillion production run of 6 designs heres a custom Tile shop I checked out a few years back and they do custom work.
They can handle your job as they fire 10 kilns 7 days a week.
The cost may be high but the quality is high
They are in Silver city New Mexico
Mark

http://www.syzygytile.com


Thank you Mark. This is just the 'jump start' I was hoping for. And you 'got it' I'm am looking for large runs of (6) different tile designs. I'll do the research to see if we can meet SYZYGY's minimum production quota. I had found an east coast china company www.marylandchina.com who offer commercial decorating (transfer imaging). They only work on white porcelain or china clay.





0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users