Posted 13 May 2012 - 01:00 PM

Lately I've been useing paper clay for my sculptural work. I have a problem with the clay developing mold I've looked on various site and have gotten several responses. Bleach , lysol, pinesol, something called thysol . With all of them there seems to be either some contraindications or people say that's the way paper clay is (Organic contents). I don't go through a bag fast enough to keep up with the mold developing and I've heard the mold itself causes health problems. Lately I've been wondering if any has ever heard of mixing fiberglass fibers to clay for reinforcement or would that be toxic during firing. Any input would be welcomed. Thx
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,509
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 13 May 2012 - 02:17 PM

Fiberglass was big in the 60s and 70s.
I still have some fibers in my studio and add it sometimes.
What kind of paper are you using to make your paper clay?
I make porcelain paper clay with paper linter fiber. I pour it onto plaster slabs and store it until I am ready to use it.
For my Raku paper clay, I usually mix a couple hundred pounds and roll out slabs immediately. Dry them and fire them.
For my terra cotta, I use the same linter fiber and sometimes take longer to use it.
It can mold. It doesn't seem too bad to me though.

I think someone on this forum mentioned putting some hydrogen peroxide into the mix.
Marcia
Marcia Selsor
0

#3 User is offline   Frederik-W Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 250
  • Joined: 02-January 12
  • Locationa distant moon of Uranus

Posted 14 May 2012 - 05:46 AM

I mixed my own terracotta paperclay and added bleach. (I read that you should do that).
I did not use it for a month or more, and when I opened the clay it was dark inside and rotten.
It smelled worse than a rotten drainpipe.

I decided it is not worth making my own. I can buy paperclay cheaply, and whatever they do in commercial mixes,
they know what they do and it lasts.
I have not started using it yet, but I will soon.

Some people seem to be (overly?) concerned about additives commercial mixes have to make it last,
some people don't like the smell of fumes it is suppose to give off when firing,
and it seems to me that some "traditionalists" or "purists" (?) just don't like it.
I would be interested to hear opinions and be corrected if I got the wrong impression.

I have heard that it is a fantastic medium for sculptural works.
You can add wet and dry parts, it is strong and lightweight.

I would like to know if it handles thermal stress better, e.g. Raku, rapid cooling/heating.

0

#4 User is offline   MichaelS Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 12
  • Joined: 26-October 10

Posted 14 May 2012 - 12:15 PM

I just make some up , roll it into 1/2 inch thick sheets and leave to dry.....rewet when I want it. it rewets real easily. I always have about 10 sheets standing on edge near the kiln
0

#5 User is offline   macdoodle Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 79
  • Joined: 08-April 11
  • LocationOrange County, CA, USA

Posted 14 May 2012 - 12:25 PM

I read if you make it with the "green" insulation from the hardware store they add borax and supposedly it wont rot, but then also your cone 10 clay is also only able to be fired to cone 6.

I bought some premade to try, it's very different to work with and it did begin to rot after a couple weeks, but its drier out here in so cal. Others say use in a week or less.

Some students have kept some dried out to re wet to use for repairs, but you need to use paper clay of the same type( shrink rate) of clay for repairs or it does not work so well ( details,details)...

It's very different to work with and the paper is good for some different effects and uses, but bad for trimming, if you prefer to throw.

http://www.paperclay.../150whatis.html
0

#6 User is offline   trina Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 371
  • Joined: 06-December 11
  • Locationspain

Posted 14 May 2012 - 02:15 PM

I just love paperclay and make my own as needed so it never really gets a chance to mold. Generally I use one roll of toilet paper to about 1 kg of white earthenware clay.

I dont have any experience raku 'ing' it generally I low fire it to about 1000C. One quality that I find get is that you can still carve, shape or drill into it easily after it has been fired.

It definately drys well and reconstitues easily. T
0

#7 User is offline   Ducky Icon

  • Newbie
  • Pip
  • View gallery
  • Group: Members
  • Posts: 4
  • Joined: 12-May 12
  • LocationWashington & California

Posted 14 May 2012 - 06:54 PM

View PostElrod, on 13 May 2012 - 10:00 AM, said:

Lately I've been useing paper clay for my sculptural work. I have a problem with the clay developing mold I've looked on various site and have gotten several responses. Bleach , lysol, pinesol, something called thysol . With all of them there seems to be either some contraindications or people say that's the way paper clay is (Organic contents). I don't go through a bag fast enough to keep up with the mold developing and I've heard the mold itself causes health problems. Lately I've been wondering if any has ever heard of mixing fiberglass fibers to clay for reinforcement or would that be toxic during firing. Any input would be welcomed. Thx


It is quite subject to rot. If the batch isn't TOO nasty (your batch does sound pretty bad) you can add some 10% bleach solution to the bag, close it up, and try again the next day. Or wear a respirator when handling it. A lot of people mix up their paper pulp, drain it, and freeze in plastic bags. Then you can mix up only what you need. Daniel Rhodes had a section in the original version of Clay & Glazes for the Potter describing the use of fiberglass as an additive, but it's really been superseded by paper clay (as others in this thread have pointed out), and it apparently itches like crazy (think: insulation). You might want to check out Rosette Gault's web site, since she holds a patent on paper clay: http://www.paperclay.../150whatis.html
0

#8 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,509
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 14 May 2012 - 07:07 PM

I think the type of paper you use has a lot to do with some properties of paper clay. Using paper with print on it causes the stinky rot because it is the ink that rots first.
Marcia Selsor


Marcia Selsor
0

#9 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 14 May 2012 - 11:40 PM

I would not worry about a little green clay mold-It burns away and dies when dry. Mold in clay shows me its got goodness going on in it. I use mine to fast for mold to grow but have used green clay with no ill effects other than
wanting to work with clay 40 years.I thought that was from the cool aid?
mark
Mark Cortright
www.liscomhillpottery.com
0

#10 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,509
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 15 May 2012 - 07:12 AM

I have gotten black mold in paper clay but that was commercially mixed.
Marcia
Marcia Selsor
0

#11 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 182
  • Joined: 08-February 12
  • LocationCalifornia

Posted 15 May 2012 - 01:43 PM

View Postmacdoodle, on 14 May 2012 - 09:25 AM, said:

I read if you make it with the "green" insulation from the hardware store they add borax and supposedly it wont rot, but then also your cone 10 clay is also only able to be fired to cone 6.


i was going to mention this to try. many people claim it won't rot if you use this blow-in cellulose attic insulation, but it'll still rot a tad if you give it time. be cautious of volume added since the borax WILL lower melting point of clay.
0

#12 User is offline   Idaho Potter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 316
  • Joined: 26-August 10
  • LocationBoise, Idaho

Posted 16 May 2012 - 07:29 PM

I recently tossed almost 50 pounds of Laguna's paper clay. I bought it a couple of years ago (or three) and ended up having surgery instead of playing with the clay. When I revisited the box of clay, it was ripe with black mold and white tufts of fuzz. I'm used to seeing green mold on old clay and don't give it a second thought but the paper clay threw me.

I emailed Laguna and asked their advice. They told me that the mold that forms on a regular ceramic clay body is part of a natural aging process, but the paper clay mold is another story. They suggested tossing what I had and to use a respirator if handling it unwrapped. I hated to throw away money, but figured my health was more important. Maybe I should have written them again to ask if it is the linter fiber that causes the toxic mold.

When I took the Graham Hay/ Rosette Gault workshop, they both recommended making thin slabs of the clay; letting it dry; and storing it that way until needed. Wish I'd remembered that before surgery intervened.
0

#13 User is offline   madi beattie Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 11
  • Joined: 16-April 12

Posted 17 May 2012 - 10:40 AM

I work only with paper clay, I make my bucket of porcelain slip then I add cheap (the cheapest i can find) toilet paper. I blend it with boiling water and a hand mixer and had it to the slip, you can play about with the amount to add to the slip. I pour it over plaster bats to create paper thin sheets. I only make enough to do me for a few days. Also there is a supplier that makes flax paper clay and it had a chemical added to it to stop it forming mould. Also if i dry out my paper clay sheets they will last for years with out mould forming. (I had a lot of dried paper clay from uni and 3 years later it was perfect to use again). I hope this helps...good luck :)
0

#14 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,509
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 17 May 2012 - 03:03 PM

I have used the blown insulation in paper clay. It worked fine.
I have also used the cellulose Green insulation from Home depot in a clay chinking mix for sealing the salt kiln door at the Bray.
It worked great.
Marcia
Marcia Selsor
0

#15 User is offline   Rohrshack Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 28-May 12
  • LocationFarmington, Connecticut

Posted 03 July 2012 - 11:06 AM

View Postmadi beattie, on 17 May 2012 - 11:40 AM, said:

I work only with paper clay, I make my bucket of porcelain slip then I add cheap (the cheapest i can find) toilet paper. I blend it with boiling water and a hand mixer and had it to the slip, you can play about with the amount to add to the slip. I pour it over plaster bats to create paper thin sheets. I only make enough to do me for a few days. Also there is a supplier that makes flax paper clay and it had a chemical added to it to stop it forming mould. Also if i dry out my paper clay sheets they will last for years with out mould forming. (I had a lot of dried paper clay from uni and 3 years later it was perfect to use again). I hope this helps...good luck :)


You said, "Also there is a supplier that makes flax paper clay and it had a chemical added to it to stop it forming mould." Could you reveal who that supplier might be? Thanks,
Rohrshack
0

#16 User is offline   Rohrshack Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 28-May 12
  • LocationFarmington, Connecticut

Posted 03 July 2012 - 11:07 AM

I am looking for a commercial supplier of white, low fire, paper clay. Any suggestions?
0

#17 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,400
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 03 July 2012 - 03:17 PM

I Googled paper clay suppliers and a lot of hits came up. A lot of the regular clay suppliers carry a paper clay body.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#18 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 03 July 2012 - 06:29 PM

I like paper clay for sculpture work
It 's hard to cut clean in slabs but you can really get away with lots of things that non paper clay will not do like huge out hangs without support while drying
like the arms in this cone 10 salt piece of mine- one of my gate demon dog series.
Mark

Posted Image
Mark Cortright
www.liscomhillpottery.com
0

#19 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 03 July 2012 - 11:31 PM

Mark, I noticed that there is a nail hole in the base of your sculpture, it needs it. You do know if allowed to be free that thing gets off of the table in the middle of the night and eats all of the meat in the house? HEY, WHERE'S THE CAT????


INRI
0

#20 User is offline   DBCurley Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 15
  • Joined: 23-June 12

Posted 04 July 2012 - 06:52 AM

While I enjoyed paper clay properties for my sculptural work, I also hated it. It was amazingly forgiving as far as drying out and re constituting it with water. My biggest issue was the cracking. It didn't seem like it enjoyed being pushed to such a large scale (1:1 human figures). I also ran into the mold issue. Usually I just uncovered the work and let some sun hit it for a while. It seemed to work fine. Mold never bothered me much...it should, but I'm poor when it comes to safety practices in studios where I get spoiled with fancy ventilation and such :P
My gallery. please visit!

"A human being should be able to change a diaper, plan an invasion, butcher a hog, conn a ship, design a building, write a sonnet,balance accounts,build a wall, set a bone, comfort the dying,take orders,giveorders,cooperate,act alone, solve equations, analyze a new problem, pitch manure, program a computer, cook a tasty meal, fight efficiently, die gallantly. Specialization is for insects." — Robert Heinlein

'....and throw a mug!' -- Brandon Curley
0

  • (2 Pages)
  • +
  • 1
  • 2
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users