So i get back from my 6 week trip, all crazy excited to get back to the studio, think 'Hey I'll just through a few little bowls'. You know just to get back into it and have something to play around wíth this weekend and I woke up this morning with my wrist a hummmmming :(

Eek who knew, trust me I was humbled....

T
P.S on a more exciting note: my art centre is having an evening with Paul Bryn Davies. He is going to a demonstrate drawing fairies and dragons. If you don't know him he has drawn the jackets for at least 15 Stephen King novels. Ya!
0

#2 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,193
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 12 May 2012 - 02:52 PM

Define humming. Like in pain? Tendonitis, carpal tunnel?
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#3 User is offline   macdoodle Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 75
  • Joined: 08-April 11
  • LocationOrange County, CA, USA

Posted 12 May 2012 - 04:42 PM

oh, i think i know that feeling; the muscle seems to be vibrating.
I have not yet decided if it should be called an ortho or neuro problem as
B-12 deficiency then muscle over use or misuse seems to set it off for me..

If you are vegetarian or vegan, pop them pills - you wont get enough from food.
http://www.healthali...vitamin-B12.php
0

#4 User is offline   trina Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 327
  • Joined: 06-December 11
  • Locationspain

Posted 13 May 2012 - 02:00 AM

Thanks guys,
I would say more like and ache generally, but with a actually pain when i extend the wrist. I am sure nothing too seriuos probably just over did it on the first day back. Have been eating marmite for some extra b vitamin. just getting older i guess.... it happens. T
0

#5 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,439
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 13 May 2012 - 05:28 AM

Beware of carpal tunnel syndrome. That is how it starts. Look up a few simple exercises to reduce the stress on the carpal tunnel.
There are some was ones. You could do tham at the wheel every 1/2 hour or so while throwing.