Posted 11 May 2012 - 08:36 AM

It seems that no matter how hard I try, my handles are always crooked on my cups. Is this because the clay is twisting and "unwinding" as it dries? If so, which direction (I can never remember)?


0

#2 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,205
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 11 May 2012 - 09:42 AM

Please describe how you are making your handles.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#3 User is offline   macdoodle Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 75
  • Joined: 08-April 11
  • LocationOrange County, CA, USA

Posted 11 May 2012 - 03:42 PM

View Postbianca, on 11 May 2012 - 05:36 AM, said:

It seems that no matter how hard I try, my handles are always crooked on my cups. Is this because the clay is twisting and "unwinding" as it dries? If so, which direction (I can never remember)?


are you doing traditional pulled handles or cutting slabs or free form?
got any pictures to show?

Is the cup base thrown or slab or hand pinched?

A very wild guess is that you are pushing the cup base clay one way and the handle clay another, since you are not saying they are also breaking off .
0

#4 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 700
  • Joined: 07-December 11
  • LocationCanada

Posted 11 May 2012 - 07:05 PM

My pulled handles used to twist to the right. This is because I am left-handed, and when I pulled the excess clay off at the bottom, I pulled the handle off centre. I now cut the excess clay off at the bottom with a fettling knife. Try it! It really works.
TJR.
0

#5 User is offline   yedrow Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 362
  • Joined: 06-February 12

Posted 11 May 2012 - 10:38 PM

Hmm, are you reversing your fingers equally when you are pulling your handles (right side then left side)? Also, sometimes it helps me to look at the 'center line' from an angle when I'm lining handels up (/ not | or -). If I look vertical or horizontal I can get things out of line, and, a look from the top (handle ~5 o'clock) is different from a look from the side. On top of that. a look from the left is different from a look from the right. Visit the handle from all perspectives. Just because its the topic: The aesthetic of your handle is like 80% negative space, not the handle.

I hope some of that was of use.
0

#6 User is offline   GMosko Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 18
  • Joined: 11-May 12
  • LocationPueblo, CO

Posted 11 May 2012 - 11:28 PM

It is my belief that the drying of the handle has nothing to so with the twisting you describe. Having seen a bit of this in the past, it caused me to examine my methods and make some changes. IMHO your "twisting" is not really a twisting at all; it is simply that you pressed the handle on crookedly.

If I make my scored and slipped areas perfectly straight, vertically, I'm half way there. Next, I always turn the mug so that the handle area is facig directly toward my face, before I press in the bottom. How else can I see if it is straight or not?

Best of luck to you.

Attached File(s)


Gil Mosko
0

#7 User is offline   Frederik-W Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 244
  • Joined: 02-January 12
  • Locationa distant moon of Uranus

Posted 11 May 2012 - 11:52 PM

The twisting is because of the centrifugal force of the earth,
and you will get a different twist depending whether you are in the southern or northern hemisphere.

Of course I'm just kidding. Just have a very straight eye when you put them on - line them up.
And if they are not perfect - it just adds more character.
Good luck.

0

#8 User is offline   INYA Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 86
  • Joined: 06-April 12
  • LocationSlovenia, Europe

Posted 12 May 2012 - 09:27 AM

Hey Mosko,

one of the best looking glazes I have ever seen!!

I am a fan of clear glazes and "minimal" pieces but yours are fantastic.
.......................

skratblog.blogspot.com
www.skrat.eu
0

#9 User is offline   yedrow Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 362
  • Joined: 06-February 12

Posted 13 May 2012 - 10:39 AM

View PostGMosko, on 11 May 2012 - 11:28 PM, said:

It is my belief that the drying of the handle has nothing to so with the twisting you describe. Having seen a bit of this in the past, it caused me to examine my methods and make some changes. IMHO your "twisting" is not really a twisting at all; it is simply that you pressed the handle on crookedly.

If I make my scored and slipped areas perfectly straight, vertically, I'm half way there. Next, I always turn the mug so that the handle area is facig directly toward my face, before I press in the bottom. How else can I see if it is straight or not?

Best of luck to you.


Is that a strait iron oxide underglaze?
0

#10 User is offline   ~janie Icon

  • ~janie
  • PipPipPip
  • Group: Members
  • Posts: 99
  • Joined: 28-July 10
  • LocationHot old Texas Coast

Posted 14 May 2012 - 04:09 PM

I sympathize with the crooked handles. I am cursed with the ugliest handles in all of potterdom.

I cannot seem to pull a decent handle- they are always crooked, too wide, too narrow, too BIG, not big enough, have thick and thin spots, or are covered with splotches of slip that I didn't see until the pot was fired. I have had very good potters try to help me with this affliction, nothing seems to help.

The thumb mug was my friend, until I decided that that was too easy, and a coward's way out. I am working on my problem, hope to resolve it one day. I do have some friends who tell me that I am far too hard on myself, that my handles are perfectly acceptable. But then they are my friends....or maybe not.

I am sorry that I cannot help you with your problem, bianca, but I do appreciate you posing this question. I would like to see a picture of what your handles.
0

#11 User is offline   Natania Hume Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 113
  • Joined: 10-July 11

Posted 16 May 2012 - 11:54 AM

I am pulling the handles, and will try cutting them off with a fettling knife, and also looking at the horizontal line, and not only the vertical one. Thanks!


0

#12 User is offline   Marry12 Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 17-May 12

Posted 17 May 2012 - 03:02 AM

View PostINYA, on 12 May 2012 - 06:27 AM, said:

Hey Mosko,

one of the best looking glazes I have ever seen!!

I am a fan of clear glazes and "minimal" pieces but yours are fantastic.


The process of production, the mood has is joyful!Posted Image
0

#13 User is offline   GMosko Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 18
  • Joined: 11-May 12
  • LocationPueblo, CO

Posted 23 April 2013 - 08:20 AM

View PostINYA, on 12 May 2012 - 07:27 AM, said:

Hey Mosko,

one of the best looking glazes I have ever seen!!

I am a fan of clear glazes and "minimal" pieces but yours are fantastic.

Gil Mosko
0

#14 User is offline   GMosko Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 18
  • Joined: 11-May 12
  • LocationPueblo, CO

Posted 23 April 2013 - 08:20 AM

Excuse me--I only just saw your comment today. Thank you! It is very kind of you to say these nice things.

Gil
Gil Mosko
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users