: Avery? -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Avery? glaze material Rate Topic: -----

#1 User is offline   carlaherren Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 28-July 10

Posted 08 May 2012 - 06:01 PM

If a receipe calls for AVERY what else can be substituted? Thanks
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,378
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 08 May 2012 - 08:48 PM

After some time with Google here is what I found
(.[1] In addition unavailability ofother materials such as Jordan clay and Avery kaolin, have brought attention tothe advantages of seeking alternate sources or distributors for ceramic glazematerials. The glaze materials areproduced for mass industrial use and its continued production and supply isdependent on continued industrial need. Despite ubiquitous use of these materials by potters and ceramists, theyare not a significant portion of the buying market and therefore have littlecontrol over the production of materials that are vital to theirprofession. In response to the unavailabilityof Gerstley borate, Jordan clay, and Avery kaolin, potters have explored use ofover the counter sources of glaze materials. In addition there has been a resurgence of interest inobtaining glaze materials and clays naturally by locating clay deposits androcks in the local environment.)

So its a koalin clay-Use EPK to start as its cheap and easy.Mark<br clear="all">



Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 08 May 2012 - 08:52 PM

Here is a reference to an Avery Kaolin . . . mined in Western North Carolina around Penland. There are other Avery slip references in ClayArt. Seems to no longer be available.

http://www.potters.o...ubject00778.htm
0

#4 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,206
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 09 May 2012 - 11:22 AM

The beauty of Avery is that it flashes very well in wood and salt kilns. EPK is a good start. If it's a small part of a recipe it probably won't make too much difference. If it's a large part, you may want to try milling it down to a finer size. Also Try Helmer Kaolin if you're making a flashing slip.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com