Posted 07 May 2012 - 11:52 PM

is it possible to make an item with holes in it, and cover those holes with
something like glaze, or glass to make it solid and transparent?
www.lotsapotsa.com
www.daddyzero.com
0

#2 User is offline   Pres Icon

  • Advanced Member
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,103
  • Joined: 02-April 10
  • LocationCentral, PA

Posted 08 May 2012 - 08:49 AM

View Postmissholly, on 07 May 2012 - 11:52 PM, said:

is it possible to make an item with holes in it, and cover those holes with
something like glaze, or glass to make it solid and transparent?


There is a technique in enameling called Plique-à-jour where a metal piece is cut out and then the enamel,basically ground glass and flux, is filled in the spaces. The piece is created resting on a metal foil or a piece of mica. After firing the piece readily releases from the mica giving a stained glass effect. Something similar is done with porcelain where carved areas coming close to piercing, but not quite are glazed with transparent glazes. I do not know of any way to do the Plique-à-jour effect on the clay, but developing such a technique may very be worth the years of effort. Maybe someone out there knows of it already being done.
0

#3 User is offline   Matt Oz Icon

  • Advanced Procrastinator
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 206
  • Joined: 16-December 11

Posted 08 May 2012 - 09:11 AM

There is an ancient technique called rice porcelain. Where small, often rice shaped holes, are cut out of the clay. When glaze fired, it creates transparent or translucent windows.

info here http://www.arabianmu...1C?OpenDocument
despite what the article says, Friedl Kjellberg is a woman.

examples from goolge images....Rice Porcelain
0

#4 User is offline   AmeriSwede Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 142
  • Joined: 01-April 10
  • LocationFörslöv, Sweden

Posted 08 May 2012 - 09:43 AM

Wow! Interesting technique, that, Matt. Thanks for that link...
I would have never suspected Arabia (Finland) rediscovered the technique. Guess the word 'rice' can be misleading.Posted Image


------Rick



Above all, it is a matter of loving art, not understanding it. (Fernand Leger
)
0

#5 User is offline   Karen.Klayworks Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 22-November 11

Posted 08 May 2012 - 01:38 PM

what a beautiful technique!
I have done this quite by accident with pierced low fired earthenware fragrance tart burners, the clear overglaze ran into and filled the pierced decorations. I really was pleasantly surprised with the effect once used when the candlelight shown through softly. No where near the beautifully delicate porcelain work on your link-

Wow, will have to keep my eye open and add one to my treasure collection when found. thanks for the link!
0

#6 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,240
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 08 May 2012 - 02:47 PM

As long as the holes are not too big, you can get them to fill in with just about any glaze. It occasionally happens on my colanders, which have 1/4 in holes.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#7 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 08 May 2012 - 02:51 PM

View Postneilestrick, on 08 May 2012 - 02:47 PM, said:

As long as the holes are not too big, you can get them to fill in with just about any glaze. It occasionally happens on my colanders, which have 1/4 in holes.


Thats why I bumped my colander hole size up a tad from 1/4 inch.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#8 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,240
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 08 May 2012 - 04:38 PM

View PostMark C., on 08 May 2012 - 01:51 PM, said:

View Postneilestrick, on 08 May 2012 - 02:47 PM, said:

As long as the holes are not too big, you can get them to fill in with just about any glaze. It occasionally happens on my colanders, which have 1/4 in holes.


Thats why I bumped my colander hole size up a tad from 1/4 inch.
Mark


Yeah, I've thought about that...
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#9 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 739
  • Joined: 07-December 11
  • LocationCanada

Posted 08 May 2012 - 07:23 PM

I ALWAYS THOUGHT THAT THOSE SMALL BLUE AND WHITE TEA BOWLS WERE MADE BY PUSHING RICE KERNALS INTO THE THIN WALLS OF A LEATHER HARD POT. THEN THE PIECE IS RAW GLAZED[NO BISQUE]. WHEN THE PIECE IS FIRED-oops, caps lock on again. When the piece is fired, the rice burns out, leaving the clear glaze to catch the light.The rice kernals are also placed in a pattern.
TJR.
0

#10 User is offline   missholly Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 158
  • Joined: 14-December 10
  • Locationzanesville, ohio

Posted 09 May 2012 - 08:19 AM

hmm....very interesting. thanks!!