White and Clear Glaze
#1
Raku
Member
Group:
Members
Posts:
16
Joined:
18-April 12
Location
Perth Western Australia
Posted
30 April 2012 - 11:56 PM
I asked a while ago for a recipe for white and clear glaze. Clay is earthenware white, temp is 1080C
Any ideas ?
Thanks
0
Back to top
MultiQuote
Reply
#2
bciskepottery
Advanced Member
Group:
Members
Posts:
753
Joined:
28-June 10
Posted
01 May 2012 - 06:08 AM
Clear Glaze, Cone 06
Silica, 2%
Ferro Frit 3134, 89.5%
Kaolin, 8.5%
Bentonite, add 2%
0
Back to top
MultiQuote
Reply
Search Topic
Forum Home
Ceramic Arts Daily Forums
|-- In the Studio
|-- Clay and Glaze Technical
|-- Business
|-- Education
|-- Aesthetics
|-- Potters Council
|-- Clay Events
← Previous Topic
Clay and Glaze Technical
Next Topic →
Page 1 of 1
You cannot start a new topic
You cannot reply to this topic
1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users