I asked a while ago for a recipe for white and clear glaze. Clay is earthenware white, temp is 1080C



Any ideas ?





Thanks
0

#2 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 01 May 2012 - 06:08 AM

Clear Glaze, Cone 06

Silica, 2%
Ferro Frit 3134, 89.5%
Kaolin, 8.5%
Bentonite, add 2%