Posted 30 April 2012 - 07:04 PM

I am looking for information on how to actually make ceramic mugs that have a built in whistle. I would like historical information on them as well "how to".
Thanks
0

#2 User is offline   atanzey Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 102
  • Joined: 02-December 10
  • LocationSouth-Central Pennsylvania

Posted 30 April 2012 - 07:29 PM

Too funny! I never would have thought to make one, but I have one somewhere that was my husband's when he was very young (late 50s, early 60s). I'll be watching to see if anyone has info on this!

Alice



0

#3 User is offline   atanzey Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 102
  • Joined: 02-December 10
  • LocationSouth-Central Pennsylvania

Posted 30 April 2012 - 07:47 PM

http://ceramicartsda...unds-with-clay/

Here's the whistle part...
0

#4 User is offline   Denice Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 449
  • Joined: 02-April 10
  • LocationWichita, Kansas

Posted 01 May 2012 - 08:29 AM

I have never heard of a whistle cup but I have made a Anazai ceremonial rattle cup, it has a hollow bottom so little balls of clay can be shaken and rattled during a ceremony. Denice
0

#5 User is offline   Mamalynx Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 24-February 12

Posted 01 May 2012 - 12:40 PM

I would be interested in hearing more about how to make these as well...

View PostDenice, on 01 May 2012 - 08:29 AM, said:

I have never heard of a whistle cup but I have made a Anazai ceremonial rattle cup, it has a hollow bottom so little balls of clay can be shaken and rattled during a ceremony. Denice