Hello, After reading much information on the web and on this forum I am still confused as to what respirator to us for spraying glaze, mixing glazes and using ferric chloride.

I just bought a mask at Home Depot that is by MSA Safety Works It says multi-purpose meets OSHA and NIOSH P100. it says for applying pesticides, working near asbestos and spraying paint. The removable cartridge has a number 4410 on it. Since I am not spraying pesticides, paint or working with asbestos I am not sure if this is a safe mask to use. I also wonder if it is safe to spray outdoors in a box without a vent. I would appreciate any information.
Thanks,

Centered
0

#2 User is offline   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 932
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 29 April 2012 - 07:26 PM

View Postcentered, on 29 April 2012 - 07:48 PM, said:

Hello, After reading much information on the web and on this forum I am still confused as to what respirator to us for spraying glaze, mixing glazes and using ferric chloride.

I just bought a mask at Home Depot that is by MSA Safety Works It says multi-purpose meets OSHA and NIOSH P100. it says for applying pesticides, working near asbestos and spraying paint. The removable cartridge has a number 4410 on it. Since I am not spraying pesticides, paint or working with asbestos I am not sure if this is a safe mask to use. I also wonder if it is safe to spray outdoors in a box without a vent. I would appreciate any information.
Thanks,

Centered


The mask is fine for spraying glazes. If outdoors why the box. I spray outdoors with the wind when there is any.
E pur si muove.

"But it does move," said Galileo under his breath.
0

#3 User is offline   Frederik-W Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 244
  • Joined: 02-January 12
  • Locationa distant moon of Uranus

Posted 01 May 2012 - 06:28 AM

If it is good enough to filter all those very horrible things, it surely is good enough for spraying glaze and the other things you want to use it for.
0

#4 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 01 May 2012 - 06:41 AM

Good info/advice on choosing respirators . . . http://www.claytimes...cles/resp2.html
0

#5 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 171
  • Joined: 08-February 12
  • LocationCalifornia

Posted 02 May 2012 - 09:56 AM

We have a EH&S Respirator Program and out of all their different types of personal filtration systems - they suggested, unless we're wearing for hours every day, that we use the disposable 3M, N95 respirators in the 8210-style. They are rated for catching the fine particulates that typically go airborne when mixing clay or glazes. We don't spray too often (because of size of work) but when we do it's inside a ventilated spray booth while wearing the mask. I believe you can sometimes find the 8210 respirators in the drywall section of some hardware stores - I always order them through a vendor like Fastenal (discount).
0

#6 User is offline   centered Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 49
  • Joined: 02-April 10

Posted 07 May 2012 - 11:37 AM

Thanks everyone for the info you provided me with.
0

#7 User is offline   nevinlee Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 11-December 12

Posted 17 December 2012 - 04:18 AM

The mask is fine for spraying glazes.Apart from that, If it is great to filter all the horrible things,then it is also great for spraying glaze as well.
____________________
online osha training
0

#8 User is offline   Round2potter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 60
  • Joined: 01-December 12
  • LocationPortland, Orygun

Posted 17 December 2012 - 04:26 PM

for a mere 17.95 you can buy a new, Finnish military surplus gas mask rated for dust and vapors! I bought mine with the specific purpose of using certain.....highly toxic, slightly radioactive, materials...

Anyway, this is way cheaper than any respirator i can find, it might look kinda scary but it would even work for the vapors coming off a soda or salt firing.

I am not sure about advertising stuff on here (as in the website to get these for cheap) so if any of ya'll want to know send me an private message.

Or iof an admin out there can tell me it is ok, ill post a link

-Burt
"There is no such thing as cheating in clay; So long as it works"
0

#9 User is offline   Diane Puckett Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 173
  • Joined: 18-July 11
  • LocationAsheville, NC

Posted 17 December 2012 - 06:54 PM

Lots of good info here
CAD Respirators for Potters

Remember to use the proper filter and change it regularly.
Diane Puckett
Dry Ridge Pottery