: Clear Glaze - White Glaze -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Clear Glaze - White Glaze

#1 User is offline   Raku Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 16
  • Joined: 18-April 12
  • LocationPerth Western Australia

Posted 27 April 2012 - 08:00 PM

Anyone got a reliable EARTHENWARE recipe for a Clear Glaze and a White Glaze. Both for functional wares.



Thanks
0

#2 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,362
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 27 April 2012 - 09:28 PM

You are asking a simple question that is incredibly tough to answer ... Closest accurate answer is ... it all depends.
What is your clay body? What temp will you be firing it to? What kind of kiln ... Oxidation or reduction?
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#3 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,429
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 28 April 2012 - 05:47 AM

If you knew the temperature (cone) and the clay body ("earthenware" covers a wide range) you could just google that. The question is too vague to answer.


Marcia

Marcia Selsor
0

#4 User is offline   Raku Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 16
  • Joined: 18-April 12
  • LocationPerth Western Australia

Posted 28 April 2012 - 06:53 PM

View PostChris Campbell, on 28 April 2012 - 10:28 AM, said:

You are asking a simple question that is incredibly tough to answer ... Closest accurate answer is ... it all depends.
What is your clay body? What temp will you be firing it to? What kind of kiln ... Oxidation or reduction?


White Earthenware, 1080C electric
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic