I've never used any stains before. I'm getting ready to start experimenting.
I've been pouring a tumbler cup mold with just plain white porcelain slip, into a plaster mold I made. If I add mason stain to the slip would it stain the plaster mold? If it does, would it effect or contaminate the next pouring w/o stain? I hope that makes sense. I just want to try and color my slip, but don't want it to ruin my plaster mold.

Thanks,
Gwen


0

#2 User is offline   INYA Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 87
  • Joined: 06-April 12
  • LocationSlovenia, Europe

Posted 24 April 2012 - 01:14 PM

View PostGwendeanne, on 24 April 2012 - 02:39 PM, said:

I've never used any stains before. I'm getting ready to start experimenting.
I've been pouring a tumbler cup mold with just plain white porcelain slip, into a plaster mold I made. If I add mason stain to the slip would it stain the plaster mold? If it does, would it effect or contaminate the next pouring w/o stain? I hope that makes sense. I just want to try and color my slip, but don't want it to ruin my plaster mold.

Thanks,
Gwen


No, it will not stain the mold.
.......................

skratblog.blogspot.com
www.skrat.eu
0

#3 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 24 April 2012 - 05:26 PM

I've had mason stain -- mixed with a porcelain slip made from clay and applied as decoration on slabs -- leave color stains on plaster hump/slump molds. I know there are body stains -- that are added to white slip for coloring -- but have not used them in molds.
0

#4 User is offline   icyone Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 65
  • Joined: 29-August 10

Posted 26 April 2012 - 03:50 AM

I think it would be best to try it on an old slip mold first. Whenever I use my red slip it stains the molds and almost everything else. So much that I use specific molds just for my redware slip.

I see you're in Colorado. If you don't have an old or extra slip mold if you want send me a message with your email or address and I'll mail one out to you. I'm in Centennial.
0

#5 User is offline   Gwendeanne Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 14
  • Joined: 09-March 11
  • LocationColorado

Posted 29 April 2012 - 08:59 AM

Thanks All. Icyone, I do have some old molds to experiment with...Thanks for offer and the heads up on the red stain. At the moment I don't have any red stain, but in the future I will be aware.