I have a bunch of type N thermocouple wire. I suspect the answer is no, but can I use this for a type K thermocouple? If not, anyone need some type N thermocouple wire, lol.
0

#2 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,490
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 24 April 2012 - 09:43 AM

Nope... it will skew the readings.

best,

...............john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#3 User is offline   yedrow Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 362
  • Joined: 06-February 12

Posted 24 April 2012 - 12:34 PM

**snaps his fingers and mumbles something better left a mumble**
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users