Posted 23 April 2012 - 09:43 AM

I need to glaze fire (^05) a few pieces for an upcoming sale, but will only have enough work to fill less than half of the kiln. What is the best placement in the kiln? I have an L&L with 3" walls. I could put everything on two shelves, but would it be better put in all the shelves and distribute the work evenly on them with only one or two pieces per shelf? If I just put everything on two shelves, is it better to have them closer to the bottom, middle or top? Thanks for any help.
Brenda Moore
Mossy Rock Creations
High Point, NC
0

#2 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,399
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 23 April 2012 - 10:24 AM

I instinctively load small batches in the middle of the kiln ... Am also curious if this is right or wrong.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#3 User is offline   Arnold Howard Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 185
  • Joined: 26-May 10
  • LocationMesquite, Texas USA

Posted 23 April 2012 - 10:59 AM

View PostMossyrock, on 23 April 2012 - 08:43 AM, said:

I need to glaze fire (^05) a few pieces for an upcoming sale, but will only have enough work to fill less than half of the kiln. What is the best placement in the kiln? I have an L&L with 3" walls. I could put everything on two shelves, but would it be better put in all the shelves and distribute the work evenly on them with only one or two pieces per shelf? If I just put everything on two shelves, is it better to have them closer to the bottom, middle or top? Thanks for any help.


I suggest loading the pieces throughout the kiln, with several pieces on each shelf.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com
0

#4 User is offline   Mossyrock Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 143
  • Joined: 22-August 10
  • LocationHigh Point, NC

Posted 23 April 2012 - 04:27 PM

Thanks for the responses. I'll load as usual just with fewer pieces. This forum is great and the people who give their help so freely are wonderful!
Brenda Moore
Mossy Rock Creations
High Point, NC
0

#5 User is offline   Idaho Potter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 316
  • Joined: 26-August 10
  • LocationBoise, Idaho

Posted 25 April 2012 - 03:54 PM

I don't usually work with low-fire glazes, but occasionally have to use low fire glazes to cover a glaze combo that didn't come out as expected. Because it's only a few pieces, I fire them on the top shelf of a bisque firing. Doesn't seem to affect the glaze and I don't feel like I'm wasting space.
0

#6 User is offline   SmartsyArtsy Icon

  • Chris Seminara
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 148
  • Joined: 29-October 11
  • LocationPNW

Posted 25 April 2012 - 05:03 PM

View PostIdaho Potter, on 25 April 2012 - 01:54 PM, said:

I don't usually work with low-fire glazes, but occasionally have to use low fire glazes to cover a glaze combo that didn't come out as expected. Because it's only a few pieces, I fire them on the top shelf of a bisque firing. Doesn't seem to affect the glaze and I don't feel like I'm wasting space.



I do the same with good results.


Chris
Chris Seminara Ceramics
Member, Artisan Tile NorthWest
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users