VC #71, or a nice satin base ? anybody using this, or have one to offer?

#1 User is offline   clay lover Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 402
  • Joined: 08-April 10

Posted 22 April 2012 - 11:12 AM

I am looking for a dependable base glaze, cone 6, that has a satin surface, nice to handle and food safe. I came across Val Cushing 71 in a book, but don't remember where I found it. Do any of you use this and do you have a good satin base that is receptive to oxides, that I might try?

I have looked up and mixed a lot of other glazes, but this is my first time to start with a base and add colorants to get what I want.

Custer spar 40
frit 3124 9
whiting 16
talc 9
epk 10
flint 16

Thanks, all.
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,444
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 22 April 2012 - 03:54 PM


This is a nice satin gloss clear that works well with stains at ^6. Hotter and it goes glossy.

Sue Hintz Clear 6^ reworked by Ron Roy back in late 90s.


Cornwall Stone 33.5

G200 22
Whiting 18
Gerstley Borate 10
EPKaolin 5.5
Silica 11
Bentonite 2


Marcia
Marcia Selsor
0

#3 User is offline   jd53 Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 18
  • Joined: 01-October 10
  • LocationNH usa

Posted 22 April 2012 - 07:55 PM

i too want to try VC 71 base, ....soon

presently i am working with john posts ( Post's calcium matte 7 )

first tests are looking good

http://www.johnpost....pes/CALMATT.TXT

http://www.johnpost....0Tiles/038.html
0

#4 User is offline   clay lover Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 402
  • Joined: 08-April 10

Posted 22 April 2012 - 08:58 PM

JD, pics look good. What does it FEEL like? The little test of VC 71 I've done with no colorants is silky, makes you want to touch it, and a bit translucent, but that might be from the lacl of colorants/ Maybe?
0

#5 User is offline   esh Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 6
  • Joined: 22-September 11

Posted 23 April 2012 - 10:56 AM

View Postclay lover, on 23 April 2012 - 03:58 AM, said:

JD, pics look good. What does it FEEL like? The little test of VC 71 I've done with no colorants is silky, makes you want to touch it, and a bit translucent, but that might be from the lacl of colorants/ Maybe?


Colorants rarely affect the glaze' texture. If you like your base glaze - just start to perform some tests using different colorants / quantities. Enjoy!
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users