: Butter Yellow Glaze -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Butter Yellow Glaze Glaze Recipes

#1 User is offline   serdwins Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 18-November 11

Posted 21 April 2012 - 04:30 PM

Looking for a cone 5-6 butter yellow glaze recipe. I would like for it to be glossy and transparent, but willing to try different types to see which one looks best.

Thanks-Sara Erdwins
0

#2 User is offline   clay lover Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 402
  • Joined: 08-April 10

Posted 22 April 2012 - 12:03 PM

Are you meaning a celadon, truely transparent?
0

#3 User is offline   serdwins Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 18-November 11

Posted 22 April 2012 - 12:44 PM

Yes a celadon glaze would work. I'm pretty new to glazing, so I'm just now learning the terminology for certain glaze types.

View Postclay lover, on 22 April 2012 - 11:03 AM, said:

Are you meaning a celadon, truely transparent?

0

#4 User is offline   serdwins Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 18-November 11

Posted 22 April 2012 - 12:54 PM

P.s. I'm working with white stoneware
0

#5 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,444
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 22 April 2012 - 03:52 PM

Does it need to be food safe?

Marcia
Marcia Selsor
0

#6 User is offline   serdwins Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 18-November 11

Posted 22 April 2012 - 10:49 PM

Nope, not necessarily.
0

#7 User is offline   esh Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 6
  • Joined: 22-September 11

Posted 23 April 2012 - 11:00 AM

See the VC #71 thread - it has a nice sample of a yellow glaze.