hi guys
i want to know about naked raku and how can i do it?
0

#2 User is offline   Raku Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 16
  • Joined: 18-April 12
  • LocationPerth Western Australia

Posted 18 April 2012 - 10:19 PM

Naked Raku



Well strip down and fire away. Dont burn your WILLY though.



What the hell is Naked Raku
0

#3 User is offline   Frederik-W Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 244
  • Joined: 02-January 12
  • Locationa distant moon of Uranus

Posted 19 April 2012 - 06:27 AM

"Naked Raku" is a desperate attempt to make Raku sound sexy.
1

#4 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,488
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 19 April 2012 - 07:30 AM

It was pioneered by Paul Soldner. He demonstrated a variation of this at many NCECA conferences ......... called "Naked Running". Posted Image

(The old folks amongst this group will likely understand this post.) Posted Image

best,

................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#5 User is offline   Denice Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 451
  • Joined: 02-April 10
  • LocationWichita, Kansas

Posted 19 April 2012 - 08:47 AM

View PostJBaymore, on 19 April 2012 - 07:30 AM, said:

It was pioneered by Paul Soldner. He demonstrated a variation of this at many NCECA conferences ......... called "Naked Running". Posted Image

(The old folks amongst this group will likely understand this post.) Posted Image

best,

................john


John maybe we should have a X-rated forum to relate Paul Soldner encounters on for the young potters on this wild man of clay. I only met him three times and each one has a story and from what I understand he was on his best behavior at the time. Denice
0

#6 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 19 April 2012 - 11:05 AM

Google Linda and Charles Riggs . . . masters of the technique.
0

#7 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,436
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 19 April 2012 - 02:55 PM

Also David Roberts from UK is another master as well as Wally Assenbergh from the Netherlands.
Linda, Charlie, Robert and Wally are all very accommodating.

Robert is the one who introduced me to Diapads when we were both teaching at the Kelowna Clayfest in British Columbia. He uses them to clean off the resist slip. The surface of his work feels like a glaze after that. I am lucky to have gotten one o his pieces.

Marcia
Marcia Selsor
0

#8 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 19 April 2012 - 03:48 PM

I was introduced to Diapads by Bill Van Gilder; that tip alone was worth the cost of the workshop. Use mine wet for cleaning up feet and bottoms after firing. I keep 100, 200, and 400 grit around.