: Old school electronic Kiln controller -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Old school electronic Kiln controller Rate Topic: -----

#1 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,360
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 06 April 2012 - 08:25 PM




Back in the day this was state of the art. It doeseverything I need which is to say it ramps up the kiln without me being present.You dial in ramp time (kiln switches are set to high) and in whatever hours you dialit will be on 100% full on in that time. The Dawson setter turns the kiln off orthe backup timer for a fail safe.

The brand is Fire right-I built this out of an old electricalbox and wired it up then mounted it next to kiln. Like a Timex its still keepsticking to this day.

Mark


Mark Cortright
www.liscomhillpottery.com
0

#2 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,199
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 07 April 2012 - 09:18 AM

We used those on the Alpine electric kilns for a long time, right up until 2003 when we switched to a touch pad controller. They worked great.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com