I'm going to be experimenting with a new glaze from John Hesselberth book and it calls for rutile. I get my supplies from the Clay Art Center in Seattle and they have two diifferent ones, one is milled ( thinking this is the one) and the other it says is "ceramic rutile", say's it should be screened before using due to various sized particles. I'm assuming that I need the milled rutile, but wanted to make sure.
Thanks for the help.
Bob
Page 1 of 1
What rutile to get?
#4
Posted 04 April 2012 - 05:12 PM
I looked up my records-I get my rutile by the 50# bag from Laguna Clay Co.
They sell 3 types
Milled
Ceramic Grade-which is plenty fine
Granular –which looks sort of darkish
I have been using ceramic grade for 30 years as I go thru lots
The brands have changed over the years but its all been ceramic grade for me.
I just check both my bags and they are really fine powder.
Your supplier may have only two kinds
Mark
They sell 3 types
Milled
Ceramic Grade-which is plenty fine
Granular –which looks sort of darkish
I have been using ceramic grade for 30 years as I go thru lots
The brands have changed over the years but its all been ceramic grade for me.
I just check both my bags and they are really fine powder.
Your supplier may have only two kinds
Mark
Mark Cortright
www.liscomhillpottery.com
www.liscomhillpottery.com
#5
Posted 05 April 2012 - 09:34 AM
Thanks for the responses. I'm looking at making a smooth glaze so the milled would work the best. But, I've also been interested in adding to a glaze to add iron spots to it. I think I will buy the ceramic grade and screen it to take out the larger pieces to use later.
Thanks again.
Bobg
Thanks again.
Bobg
#6
Posted 05 April 2012 - 10:07 AM
Bobg, on 05 April 2012 - 09:34 AM, said:
Thanks for the responses. I'm looking at making a smooth glaze so the milled would work the best. But, I've also been interested in adding to a glaze to add iron spots to it. I think I will buy the ceramic grade and screen it to take out the larger pieces to use later.
Thanks again.
Bobg
Thanks again.
Bobg
Bobg;
I don't know if you are familiar with Dansk Pottery. They make a high end stoneware dinner plate in Albany slip colour[brown] and a white matt that has speckles. They are fired in oxidation in an electric kiln. [I think]. Potters add speckles to their glazes to get that stoneware reduction effect. You can use granular rutile, and you can also use granular illmanite. Don't quote me, but I think 2% would give you the effect you are looking for.I do not use these techniques in my own work, but remember them from art school.Good luck.
TJR.
Page 1 of 1

Sign In
Register
Help










MultiQuote