But there's only one way to know for sure ... and sometimes only one way to convince a student ... let him try it!
-Mea
#6
Posted 13 June 2010 - 07:39 PM
GEP, on 09 June 2010 - 04:45 PM, said:
But there's only one way to know for sure ... and sometimes only one way to convince a student ... let him try it!
-Mea
Same problem! WHAT IS A PLATE SETTER?
#7
Posted 14 June 2010 - 10:31 PM
idale, on 13 June 2010 - 08:39 PM, said:
GEP, on 09 June 2010 - 04:45 PM, said:
But there's only one way to know for sure ... and sometimes only one way to convince a student ... let him try it!
-Mea
Same problem! WHAT IS A PLATE SETTER?
A plate setter is a "mini kiln shelf" designed to hold one plate. They have their own built-in legs, and will stack on top of each other. Depending on the situation, sometimes this is a much more space efficient way to fire plates, compared to firing them in a single layer.
I've attached a photo of 3 plate setters stacked on a 20 inch round kiln shelf. Hope this helps.
-Mea
#8
Posted 14 June 2010 - 10:34 PM
-Mea
#9
Posted 20 June 2010 - 02:51 PM
Mistelle, on 09 June 2010 - 07:49 AM, said:
Bonjour,
pour que les assiettes ne se déforment pas, je fais des anneaux dans la même terre, pour la cuisson. Cela marche parfaitement.
Bonne réussite!
Judith
Autour de la Terre
Nyon/CH
#10
Posted 20 July 2010 - 05:18 PM
Plate setters are good.
You can use uniform coils if he wants the plates off the shelf for better heat circulation. Arrange coils like sun rays, radiating out.
You can correct that the stilt would deform the plates as the plates shrink during the firing. The only way to prevent that would be to high fire bisque them and then glaze them adding gum solution to the glaze to help it stick.
For what is is worth, I'd go with plate setters or coils.
#11
Posted 20 July 2010 - 06:43 PM
Mudlark
#12
Posted 20 July 2010 - 07:29 PM
Mudlark, on 20 July 2010 - 07:43 PM, said:
Mudlark
Would wadding work for the plates then??