: Bowl stuck to support ... oh my! -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Bowl stuck to support ... oh my! Ideas to dislodge it / save it ?? Rate Topic: -----

#1 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,400
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 29 February 2012 - 05:32 PM

Here is a bowl just pulled from a Cone 6 firing.
I had supported it in another bowl form so it would not sag, but forgot to coat with kiln wash and of course the blue color fluxed and they are stuck together.<_<
Every place you can see navy blue is fluxed ... I've tried tapping it, gently trying to get under any small opening with no luck. Was thinking hot water on the bottom and ice cubes in the bowl???
Any other ideas welcomed before I do something brash!

Attached File(s)


Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#2 User is offline   Matt Oz Icon

  • Advanced Procrastinator
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 206
  • Joined: 16-December 11

Posted 29 February 2012 - 05:47 PM

When I've had similar, sometimes I'm successful pushing a thin metal rib between the two.
Best wishes
0

#3 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 29 February 2012 - 05:50 PM

I have had good luck with freezing pots in freezer and then warm/hot water on selected areas to separate them
You can tap with a wood handle while doing this-It may take several tries
You can freeze them all then invert with hot water on bowl backside running in sink
Then freeze again and try filling inner bowl only right side up with super hot water and leave outer bowl cold.
I can usually get all stuck lids off this way.
As a last ditch snap the outer bowl to free the inner-Depending if the freeze doe not work.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#4 User is offline   Pres Icon

  • Advanced Member
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,104
  • Joined: 02-April 10
  • LocationCentral, PA

Posted 29 February 2012 - 07:35 PM

View PostChris Campbell, on 29 February 2012 - 05:32 PM, said:

Here is a bowl just pulled from a Cone 6 firing.
I had supported it in another bowl form so it would not sag, but forgot to coat with kiln wash and of course the blue color fluxed and they are stuck together.<_<
Every place you can see navy blue is fluxed ... I've tried tapping it, gently trying to get under any small opening with no luck. Was thinking hot water on the bottom and ice cubes in the bowl???
Any other ideas welcomed before I do something brash!



When I first saw it I thought that it was meant to be that way. Hmmm almost makes me think of reglazing it over the edges, refiring and leaving it be. Other wise I would try soaking it in water-drying off the surfces, and freezing it in for a few days to see if the expanded water to ice frees it up.
0

#5 User is offline   MadMudder Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 50
  • Joined: 31-March 10
  • LocationMooreville, NC

Posted 29 February 2012 - 07:40 PM

Hang it on a wall and call it art.
The design is really lovely. Sorry for saying this but it is nice to see that even you can make a boo boo.
MadMudder

Remind me why I'm doing this????
-Beth Ward, Crone Potter
0

#6 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,400
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 29 February 2012 - 08:31 PM

"Sorry for saying this but it is nice to see that even you can make a boo boo."

My code is one of Mario Andretti's sayings .... If everything appears to be under control you are not going fast enough!

Dish is in the freezer ... Update in the morn!
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#7 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,557
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 29 February 2012 - 09:54 PM

View PostChris Campbell, on 29 February 2012 - 08:31 PM, said:

My code is one of Mario Andretti's sayings .... If everything appears to be under control you are not going fast enough!



Great quote Chris!!!!!! I'm gonna' steal it. Posted Image

best,

............................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#8 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,557
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 29 February 2012 - 09:59 PM

If that does not do it CHris.... try this:

Turn it upside down. Support the two of them on the spread tips of your fingers located on the colored clay bowl part. Then try tapping the underneath bigger bowl with a wooden tool and making it "ring". Do this repeatedly for a LOT of hits. Over and over and over.

The HOPE would be that the vibrations you are setting up will slowly "fracture" the very slight layer of tiny micro-globules of glassy phase material that is actually attaching the two together.

Slow and easy.

best,

.....................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#9 User is offline   Kabe Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 129
  • Joined: 11-October 11
  • LocationMo.

Posted 29 February 2012 - 10:08 PM

Hi Chris hope your bowl comes loose. Has any one tryed putting some other type of expanding material under a lid or whatever. I do not know of a product but as a carpenter I worked with MDF a lot for trimming houses out. It is sort of a pressed paper powder that they pass off as wood. Paints well but is worthless if you get it wet. a 3/4 piece of it will swell up double if it sets in some water. What would happen if some material that absorbs water like MDF powder (sawdust) was put under the bowl and allowed to swell? would it produce enough force to break it loose? has any one tried it. Beautiful design hope you can save it. Kabe
0

#10 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 29 February 2012 - 10:43 PM

Weren't you going for that look? It looks great as it is. Sometimes an accident isn't really an accident but another way to achieve what you were going for. Isn't this similar to what you wanted to do. Maybe next time you can construct the two pieces as one.

Madmudder, as for mistakes everybody makes them. If anyone says they don't make any, just wait.

INRI
0

#11 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,400
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 01 March 2012 - 11:12 AM

No joy!
It is just way too fluxed in too many places ... The bowl it is now permanently displayed in is just an awful mold form that has been fired a dozen times ... Will now be used during workshops as a 'what not to do' lesson.
And as an added bonus I learned how to separate two part epoxy after it has permanently set on something you forgot about while you were trying to get a bowl out of a bowl ......
Can't wait to see what happens next! :P
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#12 User is offline   Pres Icon

  • Advanced Member
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,104
  • Joined: 02-April 10
  • LocationCentral, PA

Posted 01 March 2012 - 11:19 AM

View PostChris Campbell, on 01 March 2012 - 11:12 AM, said:

No joy!
It is just way too fluxed in too many places ... The bowl it is now permanently displayed in is just an awful mold form that has been fired a dozen times ... Will now be used during workshops as a 'what not to do' lesson.
And as an added bonus I learned how to separate two part epoxy after it has permanently set on something you forgot about while you were trying to get a bowl out of a bowl ......
Can't wait to see what happens next! :P


Studio moments, One discovery to the next some happy some not so, but always forward-heh!
0

#13 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,400
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 01 March 2012 - 01:51 PM

Well, just so you shouldn't think the firing was a total loss ..... three junkers,( already got the hammer ), two mehs?,( might eventually meet the hammer ) and the rest not bad.;)

Attached File(s)


Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users