Posted 25 February 2012 - 11:36 PM

Hello, I need some information on a technique that is called engomes, if I'm spelling it right; it's real similar to slip decorating. Where would I get info on this, I've tried the net, but evidently I didn't spell it right, nothing came up Thanks
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,360
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 26 February 2012 - 12:10 AM

View Postalligator alley, on 25 February 2012 - 11:36 PM, said:

Hello, I need some information on a technique that is called engomes, if I'm spelling it right; it's real similar to slip decorating. Where would I get info on this, I've tried the net, but evidently I didn't spell it right, nothing came up Thanks


Google

Engobes
www.duncanshearer.co.nz/glaze/engobes.html



Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   confused_yet_curious Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 39
  • Joined: 02-January 12
  • LocationPhiladelphia

Posted 18 March 2012 - 09:59 PM

Hi,
I recently started using engomes, and it works really well. I use them for tiles and I found his redish brown looking engomes color and it's really nice. Can you keep posting about your expernce with engomes, cause I'm new at it also and I'm curious to see how you make out. Plus I found some repices and let me know if you want share some! Later!
0

#4 User is offline   AmeriSwede Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 142
  • Joined: 01-April 10
  • LocationFörslöv, Sweden

Posted 19 March 2012 - 03:53 AM

View Postconfused_yet_curious, on 19 March 2012 - 03:59 AM, said:

Hi,
I recently started using engomes, and it works really well. I use them for tiles and I found his redish brown looking engomes color and it's really nice. Can you keep posting about your expernce with engomes, cause I'm new at it also and I'm curious to see how you make out. Plus I found some repices and let me know if you want share some! Later!




My apologies in advance for correcting you here, confused_yet_curious, but a slight reiteration to Marc C's post above.....

The word 'engome' is a non-word.... the term is 'engobe'. Just so any other new ceramic interested people pick up on this, we need to teach them the correct information... better from the get-go! Posted Image The original poster had a mis-spelling of the term.

Incidentally, all of the colors on the stoneware fishhead cup pictured as my avatar, excluding the main bluish color of the fishhead, are done with engobes.




------Rick



Above all, it is a matter of loving art, not understanding it. (Fernand Leger
)
0

#5 User is offline   confused_yet_curious Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 39
  • Joined: 02-January 12
  • LocationPhiladelphia

Posted 25 March 2012 - 06:59 PM

Thanks for letting me know, but it was my auto spell. I totally understand ;)

    0

    #6 User is offline   Frederik-W Icon

    • Advanced Member
    • PipPipPip
    • Group: Members
    • Posts: 244
    • Joined: 02-January 12
    • Locationa distant moon of Uranus

    Posted 02 April 2012 - 08:19 AM

    Engomes are gnomes with cute little hats and long ears that run around naked in the forest.
    They make beautiful little earthenware pots that they pit-fire, but only on Wednesdays.
    They are very rare and hard to find.

    Engobes are something completely different.

    :)
    0

    #7 User is offline   AmeriSwede Icon

    • Advanced Member
    • PipPipPip
    • Group: Members
    • Posts: 142
    • Joined: 01-April 10
    • LocationFörslöv, Sweden

    Posted 02 April 2012 - 12:33 PM

    View PostFrederik-W, on 02 April 2012 - 03:19 PM, said:

    Engomes are gnomes with cute little hats and long ears that run around naked in the forest.
    They make beautiful little earthenware pots that they pit-fire, but only on Wednesdays.
    They are very rare and hard to find.

    Engobes are something completely different.

    :)





    Posted Image Don't they call those little earthenware pots....'ceramic thimbles'....Posted Image


    ------Rick



    Above all, it is a matter of loving art, not understanding it. (Fernand Leger
    )
    0

    Page 1 of 1
    • You cannot start a new topic
    • You cannot reply to this topic

    1 User(s) are reading this topic
    0 members, 1 guests, 0 anonymous users