Art fair season is fast approaching. Acceptances and rejections have been coming in this week. Soon it will be time to re-seal my popup canopy to keep it water tight. Any recommendations?
Page 1 of 1
Sealer for Art Fair Canopy
#2
Posted 10 February 2012 - 01:07 PM
I haven't tried this myself, but I hear that lots of artists use sealers made for camping tents. It's not expensive and very effective when applied once a year. You can also pack a roll of white duct tape for temporary patches during a show.
Mea
Mea
#5
#7
Posted 10 February 2012 - 05:16 PM
I sprayed it to the outside-on a warm day after washing it a few days before lightly with a hose.
I do my two boat covers with it ever 3 years the same way
You should most likely test it on a small spot first
All fabrics are treated differently.
Mark
I do my two boat covers with it ever 3 years the same way
You should most likely test it on a small spot first
All fabrics are treated differently.
Mark
Mark Cortright
www.liscomhillpottery.com
www.liscomhillpottery.com
#8
Posted 10 February 2012 - 05:48 PM
Thanks Mark. I think that's exactly what I need. I got into a massive downpour at a fair last year, but my booth was brand new. Many of my neighbors had old booths that were not sealed, and they were a mess. Some had water inside picture frames and lost a lot of work. My pots don't mind getting wet, but I do!
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com
neil@neilestrickgallery.com
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com
neil@neilestrickgallery.com
Page 1 of 1

Sign In
Register
Help











MultiQuote