Today, when I fired these objects, two of the terra cotta objects exploded to pieces and so did one of the while clay objects. Again, these pieces ranged in size, but very small. I fired according to the kiln directions: fire to 500 degrees with a stilt propping open the hood, then removed the stilt to fire to 1950 degrees, cool to 1500 degrees and fire to 1950 degrees. At about 700 degrees, the first explosion happened, which was a small barely audible pop sound. At about 800 degrees the same sound again, so I turned it off and unplugged it. As it was cooling, there was a louder explosion, which caused "smoke" or clay powder to exhaust from the top of the kiln hood. Then, luckily nothing else happened.

One piece was completely shattered, made of terra cotta and the thickest of the pieces. Another had pieces that had exploded off of it. The last, a piece that was an inch long and a quarter of an inch think sheared in half length wise and broke apart.
All of the pieces seemed dry. Not sure what happened. Seems to me that it is most likely a combination of the drying not being complete and the kiln. (I'm going to be purchasing an electric digital kiln soon, which I hope will help with part of the problem.)
So, is there a good way to dry clay? How long should it dry for? I've heard that putting clay in a regular oven can help with drying...is that true?
Thanks for the help!