can anyone tell me if they know , earthenware or stoneware, fired to the same temp., ^06, which will be most durable?
Page 1 of 1
Again, Earthenware Vs Stoneware
#2
Posted 12 May 2010 - 09:07 AM
savant, on 12 May 2010 - 05:18 AM, said:
can anyone tell me if they know , earthenware or stoneware, fired to the same temp., ^06, which will be most durable?
Earthenware is usually most durable ^04, Stoneware at least ^6 I would assume the earthenware would be because it's closer to it maturation temperature.