Riggs Terra Sigillata Recipe for Raku

Riggs Terra Sigillata
Raku
Glaze Material
Percentage
Water 3.5 Gal
Sodium Silicate 1 tbsp
Soda Ash 1 tbsp
XX Saggar Clay 115 lbs
Mix ingredients and allow to sit and separate into sections. Gently siphon out only the middle section for use.