Hasselle Copper Matt Raku Glaze Recipe

by Holly Goring Read Comments (0)

Hasselle Copper Matt
Raku
Glaze Material
Percentage
Black Copper Oxide 80%
Ball Clay 20
  100%
Add: Bentonite 3%

This recipe is included in 10 Tried and True Raku Glaze Recipes: Recipe Cards for our Favorite Raku Pottery Ceramic Glazes, which is free to Ceramic Arts Daily subscribers.