- Ceramic Arts Daily - http://ceramicartsdaily.org -

Alligator Matt White Raku Glaze Recipe

Alligator Matt White
Raku, cone 05
Glaze Material
Percentage
Bone Ash 29%
Gerstley Borate 57
Nepheline Syenite 14
100%