Alligator Matt White Raku Glaze Recipe

by Holly Goring Read Comments (0)


Alligator Matt White
Raku, cone 05
Glaze Material
Percentage
Bone Ash
29%
Gerstley Borate 57
Nepheline Syenite
14

100%