Eggshell Glaze Recipe, Cone 6, oxidation

Eggshell Glaze Cone 6, oxidation
Glaze Material
Whiting 9.5%
Zinc Oxide 5.5%
Ferro Frit 3124 44.5%
Custer Feldspar 20.0%
Bentonite 7.5%
Edgar Plastic Kaolin (EPK) 5.0%
Silica (Flint) 8.0%
Total: 100.0%
Add:
Tin Oxide 9.0%
Red Iron Oxide 3.0%