June 1, 2009
White Crackle Glaze Recipe, Cone 06 oxidation
![]() |
|
|
From Ramon Camarillo, Ceramics Monthly, April 2002. |
||
|
This recipe is included in 10 Tried and True Low Fire Glaze Recipes: Recipe Cards for our Favorite Low Fire Ceramic Glazes, which is free to Ceramic Arts Daily subscribers.
|
||