Top Crater Glaze Recipe
Cone 08-04 Oxidation
Glaze Material
Percentage
Frit 3134 (Ferro)
52.1%
Edgar Plastic Kaolin (EPK) 11.1
Silica (Flint)
36.8
Total 100%
Add:
Silicon Carbide (100 mesh)
 1%

From James Haggerty, Ceramics Monthly, November 2005.