Red Green Glaze Recipe, Cone 06 oxidation

by Jessica Knapp Read Comments (0)

Red Green Glaze Recipe
Cone 06 Oxidation
Glaze Material
Percentage
Frit 3134 (Ferro)
50%
Custer Feldspar
50
Total 100%
Add:
Copper Carbonate 3.2%

From Ramon Camarillo, Ceramics Monthly, April 2002.