Majolica Overglaze Glaze Recipe, Cone 06-04 oxidation

Majolica Overglaze Glaze Recipe
Cone 06-04 Oxidation
Glaze Material
Frit 3124 (Ferro) 50%
Wollastonite 10
Glaze Stain  40
Total 100.0%