Be sure to download your free copy of 10 Tried and True Low Fire Glaze Recipes: Recipe Cards for our Favorite Low Fire Ceramic Glazes, a perfect resource for potters and ceramic artists who are ready to experiment with custom glazes, or for those who have grown tired of their own tried and true glazes.

May 20, 2009

Majolica Overglaze Glaze Recipe, Cone 06-04 oxidation

by Jessica Knapp Read Comments (0)

Majolica Overglaze Glaze Recipe
Cone 06-04 Oxidation
Glaze Material
Percentage
Frit 3124 (Ferro)
50%
Wollastonite 10
Glaze Stain
 40
Total 100.0%


 



Can be used over a similarly colored Matt Glaze (above) to intensify the color while retaining the matt surface.
From Sandra Luehrsen, Ceramics Monthly, June 2002.

This recipe is included in 10 Tried and True Low Fire Glaze Recipes: Recipe Cards for our Favorite Low Fire Ceramic Glazes, which is free to Ceramic Arts Daily subscribers.

 

Tags: ,

Share this post with other ceramic artists:
These icons link to social bookmarking sites where readers can share and discover new web pages.
  • TwitThis
  • Facebook
  • Digg
  • del.icio.us
  • MySpace
  • StumbleUpon
  • Google Bookmarks

You must be logged in to post a comment.