Mid-Range Reduction Firing: It’s Not Just Cooler, It’s Cool!
|
These tumblers by Erik Haagenson are an example of a nice Cone 6 reduction Temmoku |
As I have mentioned before in this blog, ceramics is not the greenest of art forms, but it is nice to know that, with a little effort, potters can reduce their carbon footprints. One way to do this is to reduce your firing temperature. But what if you are hooked on high-fire reduction firing? Erik Haagensen and Luba Sharapan, the owners of MudFire Clayworks and Gallery, had started to fire cone 6 reduction because of a defect in the kiln they’d purchased, but after seeing the results they had no reason to change back, even after the kiln was repaired. As John Britt points out in the following excerpt from Ceramics Monthly, firing to cone 6 is cheaper, faster, and the results are almost indistinguishable from high fire. - Jennifer Harnetty, editor. |
|
Making the Switch Also, there is an underlying belief, although it is completely incorrect, that cone 10 is superior to mid-range or low-fire, and changing this mind set is an educational challenge. I think that this comes from the long historical European search to imitate Chinese high-fire porcelain. The goal was always to achieve high fire, so it gained the psychological high ground. I don’t recommend converting glazes to the lower temperature, because when you lower the firing temperature of a glaze you are using different fluxing oxides that have different color responses. So although it is possible to convert your glaze to the lower temperature, you will end up with a different glaze anyway. It is better to use the many tried and true mid-range glazes already in use and test them in your cycle. This is the same way potters find high-fire glazes; they get glaze recipes from books or from friends and then vary the colorants and opacifiers. Although change is hard, potters should focus on the benefits of firing mid-range reduction. First, as stated above, it saves fuel, reduces your carbon footprint and costs less. Second, it saves time. It may take 2-4 hours to get the extra temperature of cone 10 and maybe longer depending on the size of the kiln. So rather than firing for 10-12 hours you will be out in 8-10 hours. Firing to mid-range also reduces the wear and tear on your kiln, which means that it lasts longer. Finally, and most importantly, you get great results! |
|||||||||||||||||||||||||||||||||||||||||||||||||||
|
*Malcolm Davis Shino (shown above) is one of the glaze recipes included |
|||||||||||||||||||||||||||||||||||||||||||||||||||
|
|
||||||||||||||||||||||||||||||||||||||||||||||||||
|
Mid-Range Fluxes
Glazes contain alumina and silica, which both melt at very high temperatures, so getting them to melt at mid-range temperatures requires different fluxes than at high-fire temperatures: Sodium Oxide (Na20) is a strong alkaline flux and creates brightly colored glazes. It has a melting point of 1652°F (900°C) and a high expansion/contraction rate, which will often cause crazing in glazes. It is often found in association with potassium oxide in feldspars. Common mid-range sources include sodium feldspars (nepheline syenite-actually a feldspathoid-is the lowest melting feldspar and so it is often used at midrange. It is high in sodium and lower in silica than other feldspars and melts around cone 6.), soda ash, wood ash, borax, frits and Gerstley borate or its substitutes. Lithium Oxide (Li2O) is the lightest weight, smallest particle size and most powerful of the alkaline fluxes with a strong color response similar to sodium and potassium oxides. It has a melting point of 1472°F (800°C) and has a low expansion/contraction rate, which can cause shivering in glazes. Sources include lithium feldspars and lithium carbonate. Zinc Oxide (ZnO) is an auxiliary flux in oxidizing atmospheres. It has a dramatic color response, both good and bad, depending on the colorant. It can heighten colors with copper and cobalt oxides, but produces dull colors with chrome oxide. It has a melting point of 3587°F (1975°C), but if it is fired in reduction it will change to the metal zinc and volatilize at 1742°F (950°C). It has a low expansion/contraction rate, so it can help to reduce crazing. Sources include zinc oxide and calcined zinc oxide. Boron Oxide (B2O3) is a glass former and a flux with a molecular structure similar to alumina. It melts at 1292°F (700°C) but begins melting at 572°F (300°C). It has a low expansion/contraction rate and produces good color response in glazes, with characteristic bluish, milky streaks and cloudy effects. Sources include Gerstley borate (or its substitutes like Gillespie Borate, Murray’s Borate, Laguna Borate, etc.), borax and frits. NOTE: Frits come in a wide range of types. They are used by industry as reliable and consistent sources of fluxing oxides in relatively insoluble form. They are relatively low in alumina and silica and are active melters, but they can settle rapidly. |
|||||||||||||||||||||||||||||||||||||||||||||||||||
Tags: Ceramics Monthly Master Class, Gas Kiln Firing, glaze chemistry, High Fire Glaze Recipes, John Britt, Mid Range Glaze Recipes, sustainability











Vicki | June 3rd, 2009 at 7:15 pm
Hey John
I just found this website.. WOW!!
Is the Panama Red glaze food safe?
pj | June 25th, 2009 at 6:49 am
John how do I find out more about cone 6 reduction firings? I have a olympic kiln and was told I could do cone 6 reductions in it. Is there a book or article to tell me exactly how to do this process? It seems you have to have different glazes to make it work from what I read in this article. I would appreciate and help you could give me. Thanks, pj
Jessica | July 1st, 2009 at 10:39 am
Looking for the answer to the question above: Is the Panama Red glaze food safe? Thanks
Judy | July 5th, 2009 at 11:46 am
I would also like an answer to the 2 above questions. Is this the corrected version of the recipe? I remember that the first printing was incorrect and the corrected version was in the next Ceramics Monthly magazine.
Mary Ann | July 12th, 2009 at 2:09 am
I would also like to know if the Panama Red Glaze (cone 6) is food safe?
Thanks,
MAD
Jennifer | August 19th, 2009 at 8:43 am
Because of the many variables involved in glazes (clay body and glaze fit, variability in chemical content, temperature variability in kilns, organic materials, etc.), we cannot guarantee food safety on the recipes posted on Ceramic Arts Daily. The best way to be certain is to have one of your finished pieces leach tested by a lab.
Glaze Testing Resources:
http://www.digitalfire.com/services/consultants/index.php
http://digitalfire.com/services/database.php?list=labs
Colleen | August 27th, 2009 at 6:33 pm
I made the Panama Red as printed above and got a pretty minty green????
What did I do or is Judy right and there is an error?
A B | September 2nd, 2009 at 10:56 am
We fired it and got a nice red, remember it has to have reduction to get the red.
In oxidation this is a beautiful transparent pale green.
Colleen | September 28th, 2009 at 10:48 pm
Thanks AB- I am still pretty new to all of this. Does anyone have a recipe that would be somewhat red?(cone 6 ox)From everything I have tried…..I have all sorts of greens…lol…Am I asking the impossible?
laura | October 16th, 2009 at 12:32 pm
love to have cone 6 oxidation red or great blue email lkeene@mris.com thanks
Marlene | December 13th, 2009 at 10:57 am
Dear Colleen, I see that your post is from September, so you may have already gotten the answer to this… the red happens as a result of reducing the oxygen starting at about cone 08 or 1737 degrees F.. this is one of the reasons why copper reds have long been considered so elusive.. at that point the flame becomes so hungry for oxygen that it pulls it out of the glaze and clay body.. turning the copper to red! If the reduction doesn’t happen at that point then one doesn’t get red and maybe gets green.. depending on the glaze ingredients..
Michael | January 3rd, 2010 at 5:44 pm
Hi…today i mixed a batch of Johns shino and when i printed out the recipe my printer printed it in black and white…i know i printed it from this website but i cant find that pic of the vase with it to see what it will look like….anyone? Johns shino? its a vase with underglaze birds on it…cant find it! help :(
Gary | January 31st, 2010 at 12:26 am
Is chemistry still taught in school? Copper oxidation = Green. Copper reduction = Red. I have to admit I haven’t been involved in ceramics for 25 years. Had a studio and gallery for 15 years. 60 cu/ft hardbrick, crossdraft, gas fired kiln with wood side port for extra glaze effects.
This is the first time in all these years that I have looked into what people are doing these days. I have to admit I’m a little disappointed.
I had a subscription to CM back in those days, and when someone gave me a recent edition I was sorry to find that not much has changed since then.
The only difference seems to be that no one learns where their materials come from. I had a professor and an Ozark cottage potter as my mentors.
Please don’t let the science of pottery be lost. Learn your chemistry. Learn where the materials come from and how they work together.
I hope that I’m not expecting too much from today’s potters. Gary
Kathy | March 11th, 2010 at 10:07 pm
Colleen, you can get a c/6 oxidation red using a combination of chrome and tin instead of copper. There are recipes out there, but I don’t know if I can plug any books or other websites here, so I won’t. Search the web for Lana’s Red; it’s my favorite c/6 ox red so far.
Kathy