In today’s video, I am sharing a clip (and a recipe) from John Britt’s best-selling video Understanding Glazes. In this (much-condensed) clip, John shares his simple system for mixing up a color blend and tells us what to make of the results. Have a look and then mix up your own color blend and see what you get. – Jennifer Harnetty, editor.



Having trouble watching the video? Please see our Video FAQ to troubleshoot.

This clip was excerpted from Understanding Glazes: How to Test, Tweak, and Perfect Your Glazes, which is available in the Ceramic Arts Daily Bookstore!

Order online and get free shipping!
(Free shipping applies to U.S. orders only)


For a limited time, buy Understanding Glazes for $20 off, and get a free copy of the Ceramic Arts Handbook Glazes and Glazing, to boot!


Remember: Glazing results can vary, so mix up your own color blend using this 5X20 glaze recipe and the following colorants, and see what you get!


1) Base only

2) Yellow Iron 2 %

3) Red Iron Oxide 3% & Titanium Dioxide 4 %.

4) Rutile 4 % and Cobalt Carbonate 1 %.

5) Zircopax 7%. 6) Chrome oxide 0.5%.

7) Copper Carbonate 3.5 %

8) Chrome 0.2 % and Tin Oxide 7.5 %.

9) Cobalt Carbonate 0.75 %.

10) Any stain 6 %.