emerging_620The May 2014 issue of Ceramics Monthly is out, and with it the ever popular Emerging Artists feature. 2014’s crop of artists includes 14 potters and sculptors.

 

In today’s post, two of them share the glaze recipes they use to make their fresh and interesting work- Jennifer Harnetty, editor.

 


 

Lauren Mabry and Bill Wilkey, two of our 2014 Emerging Artists, share their recipes for high-fire slips and glazes below. To see more from each of them, and the rest of this year’s Emerging Artists, check out the May 2014 issue of Ceramics Monthly (on newsstands now! Or get CM for your tablet!).

 


 

Glaze Recipes Every Month

If you enjoy trying out new glazes, check out each issue of Ceramics Monthly. For more than 60 years, Ceramics Monthly has delivered more recipes, more technical information, more ceramic art and more captivating stories about ceramic artists than any other ceramic art magazine in the world.  Check it out

 

 


Mabry_700px

 

 

Cracked Cylinder, 28 in. (71 cm) in width, red earthenware, slips, glaze, 2013. Photo by Colin Conces.

Lauren Mabry’s Cracked Cylinder, 28 in. (71 cm) in width, red earthenware, slips, glaze, 2013. Photo by Colin Conces.

 

Wilkey_700px

 

Diner mugs, 4 in. (10 cm) in height, wheel-thrown and altered porcelaneous stoneware, flashing slips, glazes, wood fired in an Anagama for 30 hours to cone 12, 2013.

Bill Wilkey’s Diner mugs, 4 in. (10 cm) in height, wheel-thrown and altered porcelaneous stoneware, flashing slips, glazes, wood fired in an Anagama for 30 hours to cone 12, 2013.

 

 


 