A Super Simple Analogy to Help You Understand Glaze Structure

Ceramic glazes consist of three main components: glass formers, fluxes, and refractories. If you can remember those, and familiarize yourself with the characteristics of the common ceramic raw materials, you are in good shape to start developing your own successful glazes. 

 

For today’s video, I thought I would share John Britt’s simple glaze component analogy. It is a great way to remember how the three glaze components function in a glaze. – Jennifer Harnetty, editor.

 


 

 

Having trouble watching the video?

Please see our Video FAQ to troubleshoot.

 

 



This clip was excerpted from Understanding Glazes, which is available in the Ceramic Arts Daily Bookstore!

Order online and get free shipping!
(Free shipping applies to U.S. orders only)

 


To learn more about John Britt or to see more images of his work, please visit www.johnbrittpottery.com.

 

For some great glaze recipes to experiment with, be sure to download your free copy of
33 Tried and True Ceramic Glaze Recipes.