How to Make Paper Stencils in Bulk
I love working with paper stencils and underglazes. There’s something so satisfying about removing the stencil to see your crisp design below. But I haven’t found an easy way to make multiples of more complicated stencils – until now. In today’s post, an excerpt from the November 2012 issue of Ceramics Monthly, Zygote Blum shares how he makes stencils in bulk – 48 or so at a time using a jeweler’s saw and frame and some other basic supplies.