Circular Logic: Using Balloons as Molds for Spherical Handbuilt Ceramic Sculpture

Posted On May 6, 2009 5 Comments

Today ceramic artist Ursula Goebels-Ellis explains how she uses balloons to create her

spherical sculptures. She also shares a clay body recipe that she

tweaked to work perfectly for this technique.