jiggering; jolleying

Posted On December 8, 2008 0 Comments
A partially mechanized vessel-forming process on the potter’s wheel, where a pivoting arm (a jigger or jolley) with a mounted profile rib is brought down against a centered clay ball within or upon a wheel-mounted mold. Source: Clay: A Studio Handbook

Jasper ware

Posted On December 8, 2008 0 Comments
Ware developed by Wedgwood in which colored stoneware is decorated with contrasting raised relief slip or clay imagery. Source: Clay: A Studio Handbook