The Irresistible Surface: Layering Glazes and Trapping Carbon to Create Loosely Geometric Repeating Patterns

Posted On August 11, 2010 13 Comments

Peter Karner developed his surface decoration through years of trial and error and he continues to try new things so that his surfaces continue to evolve. In today’s post, Peter explains how intuition combined with experimentation helped him perfect his beautiful glaze surfaces. Plus he details how he uses wax resist and layers of five different glazes to develop his gorgeous glaze patterning.