Raku on the Walls: How to Make a Raku Mural

Posted On October 8, 2014 18 Comments

If you have ever done raku firing, you are probably aware that the raku firing process should not be used for pots that are intended to serve food. The rapid firing, removal of the ware at the red-heat stage, and subsequent post-firing all contribute to surfaces that remain porous after firing. So it is best for decorative pots or sculpture. If you are looking for another application for raku, today’s post just might be for you.